3mm PETG (Polyethylene terephthalate glycol) Plastic Welding Rod Hot Air/Hot Gas Welding of PETG sheets: The welding temperature should be 120C° to 160°C. When using hot air welding it is mandatory to pre dry the sheet and the filler wire 12 hours at 60°C to avoid moisture bubbles in the welding area.
Recommended Temperatures for Hot Gas Welding:-
* Oxidisation of the matching material & welding occurs when air is used as the welding medium. • Important Note: The temperatures shown above are not the heat gun settings. They are the required temperatures that must come out of the heat gun nozzle in order to achieve a successful weld. Features:
Please Note: The data provided falls within the normal range of product properties. However, they should not be used to establish specification limits nor used alone as the basis of design. Barnes Plastic Welding Equipment Limited assumes no responsibility for any advice provided by it or for results obtained with respect to these products. All such advice is provided free and the buyer assumes sole responsibility for the results obtained in reliance thereon. |